Top bond on 15
Shot through aft inspection hole on starboard side shining on port joggle.
Redux use was pretty much identical to what we used bonding top on Klause's:
One 75 grams, (Yellow) for wetting out
Two 100 grams mixed with flox
One 50 gram mixed with flox
One 50 gram not used and went back in can.
Y9-05-02