Date: 12/31/1969 Views: 2694
Date: 04/28/2007 Views: 3622
Date: 10/24/2009 Views: 4010
Date: 08/23/2023 Views: 159976
"STARBOARD" stabilator gets packaging tape on "BOTTOM" surface at root, then applied Expancel/Aeropoxy nice and thick on wet out surface of fuse profile after it was scuff sanded with 80 grit. Y9-07-13