Holes are only 1/16" to allow proper countersinking of top tang.
Date: 10/12/2009
Views: 3813
Newest Image
EAA SITE
Date: 08/23/2023
Views: 202135
DoorLatch71Ann
Mixed FLOX into the Araldite to make a thicker, stronger bonding agent. Drilled the injection holes in the door frames. Filled the industrial syringe with the mix and injected half into each door to hold the guides.